A comparative study on direct Cu–Cu bonding methodologies for copper pillar bumped flip-chips

Y. Ma, A. Roshanghias, A. Binder

    Research output: Contribution to journalArticlepeer-review

    Abstract

    Copper pillar micro bump is one of the platform technologies, which is essentially required for 2.5D/3D chip stacking and high-density electronic components. In this study, Cu–Cu direct thermo-compression bonding (TCB) and anisotropic conductive paste (ACP) bonding methods are proposed for Ø 100 µm Cu-pillar bumped flip-chips. The process parameters including bonding temperature, bonding pressure and time are verified by die shear test and SEM/EDX cross-sectional analysis. The optimal bonding condition for TCB with regards to bonding pressure was defined to be 0.5N/bump at 300 °C or 0.3N/bump at 360 °C. In the case of ACP bonding, the minimum bonding pressure was about 0.3N/bump for gaining a seamless bonding interface.
    Original languageEnglish
    Pages (from-to)9347-9353
    Number of pages7
    JournalJournal of Materials Science: Materials in Electronics
    Volume29
    Issue number11
    DOIs
    Publication statusPublished - 28 Mar 2018

    Fingerprint

    Dive into the research topics of 'A comparative study on direct Cu–Cu bonding methodologies for copper pillar bumped flip-chips'. Together they form a unique fingerprint.

    Cite this